Upper cheek plates protect both frame sidewalls in the upper crushing chamber from material wear. The part numbers below identify Metso Nordberg C Series jaw crusher parts and require confirmation against the installed machine.

سلسلة المعدات

Metso Nordberg C Series الكسارات الفكية

Applicable Models

C80 وC96 وC100 وC106 وC110 وC120 وC125 وC130 وC140 وC150 وC200 وC3054

Part Type

Upper cheek plate

Part identification

Metso equipment and part specifications

Upper cheek plate part numbers

ModelPart NumberDescription
C100446121Cheek plate upper
C125949648704900CHEEK PLATE, UPPER
C140930654CHEEK PLATE, UPPER
418609CHEEK PLATE, UPPER
C106570392CHEEK PLATE, UPPER,C105/C106
C120MM1028794CHEEK PLATE, UPPER,XT710
C130MM0242228CHEEK PLATE, UPPER
C150MM0586529CHEEK PLATE, UPPER,C150
C200917296CHEEK PLATE, UPPER,C200
917307CHEEK PLATE, UPPER,C200
MM1236621Upper cheek plate
MM1236623Upper cheek plate
MM1236625Upper cheek plate
C3054585352CHEEK PLATE, UPPER
585353CHEEK PLATE, UPPER

أرقام القطع هي مراجع تحديد لماكينات سلسلة C من Metso Nordberg. أكِّد اللوحة الاسمية للمعدات والرقم التسلسلي والرسم قبل الطلب.

المواد والعمليات

Review the following upper cheek plate material and process information when assessing specifications and alternatives.

XT710 manganese steel

Verify cheek plate material against the specific part drawing and material certificate. The XT710 designation alone does not establish composition, hardness or interchangeability with jaw plates.

Mn13Cr2 / Mn18Cr2

Mn13Cr2 and Mn18Cr2 are candidate chromium-bearing manganese steel grades. Confirm composition, heat treatment and suitability against the drawing, material standard and actual loading.

Installation

Cheek plates are bolted to the frame sidewalls; some models use a recessed mounting arrangement.

Wear and Replacement Criteria

Use the following upper cheek plate wear patterns and replacement considerations during maintenance.

Main wear zones

Material flow zones along the middle and upper chamber sidewalls, and around bolt holes. Upper cheek plate wear is generally lighter than lower cheek plate wear.

Replacement Criteria

Assess remaining thickness against the model-specific maintenance limits. Stop and inspect if there is wear-through, cracking or loosening caused by bolt-hole wear.

Recommended Actions

Measure thickness and check bolt tightness regularly. Schedule upper and lower cheek plate replacement according to actual wear and model-specific maintenance requirements.

Information Needed for an Inquiry

المعدات model, such as C106; part number; material requirements; left/right and upper/lower position; and quantity.

خدمات صنع في الصين

من التقييم الفني إلى تسليم المنتج بالكامل

توفر شركة ANRANST للعملاء العالميين تقييمات هندسية، واختيار التصنيع الصيني، ومراقبة الجودة، وتسليم الأجزاء النهائية لقطع الغيار الصناعية المقاومة للتآكل حسب الطلب، ويمكنها أيضًا دعم قطع الغيار الصناعية الأخرى حسب الطلب.

01

مراجعة الرسومات والهندسة

قم بمراجعة أسطح التزاوج وأبعاد الواجهة، وقم بتقييم جدوى المواد والمعالجة الحرارية والتصنيع.

02

تحديد المادة والمعالجة الحرارية

تُحدَّد درجات المواد وعمليات المعالجة الحرارية لكل طلب على حدة، وتُثبَّت في الاتفاقية الفنية وتُتابَع أثناء الإنتاج.

03

ضبط الجودة

يشمل ذلك تأكيد الرسم، ومراقبة المواد والعمليات، وتتبع الإنتاج، وتنسيق عمليات الفحص والقبول.

04

تسليم المنتج النهائي

تنظيم عمليات التصنيع والتحقق من الجودة والتعبئة والتغليف وتسليم المنتجات النهائية الكاملة لتشكيل حلقة إمداد قابلة للتنفيذ.

قم بتزويدنا بالنماذج الحالية، والرسومات، وأرقام الرسومات، وأرقام الأجزاء، والمواد، أو معلومات ظروف التشغيل، وسنقوم بتحديد التحقق الفني ومسار التوريد وفقًا لذلك.

إرسال طلب